Specializing in the production of silicon carbide rods, silicon carbide rod protection tubes, silicon carbide protection tubes, sillimanite products, thermocouple protection tubes and other types, hundreds of specifications and other products. The experience of using silicon carbide rods for many years is summarized as follows:
Operating temperature: The higher the temperature of the silicon carbide rod, the shorter the life. Especially when the furnace temperature exceeds 1600°C, the oxidation speed will increase and the service life of the silicon carbide rod will be shortened. Therefore, please try not to make the surface temperature of the silicon carbide rod too high, that is, it is necessary to reduce the difference between the furnace temperature and the temperature of the silicon carbide rod.
Surface load: The surface load density refers to the allowable rated power per unit surface area of the heating part of the rod.
Surface load density = rated power (W) / surface area of heating part (cm2)
Practice has proved that the difference between the surface temperature of the heating element and the furnace temperature is also large when the load density is large. If the load density is large, the surface temperature of the rod body will be high, the resistance will increase rapidly, and the life of the SIC rod will be short. Therefore, the surface temperature load density of the silicon carbide rod, the atmosphere in the furnace, and the temperature are directly proportional to the aging rate of the SIC rod, and inversely proportional to the life of the SIC rod.
Furnace atmosphere: during firing, the silicon carbide rods will react with many chemical substances emitted from the fired products. If it reacts with water, hydrogen, nitrogen, sulfur, halogen and other gases, molten aluminum, alkali, salt, etc. If molten metal and metal oxide come into contact, reaction, corrosion or oxidation will also occur.
Kiln operation mode: In continuous furnace and intermittent furnace, silicon carbide rods have a longer life span. The surface of the silicon carbide rod is oxidized to form a silicon dioxide film during use. Long-term use will increase the silicon dioxide film and the resistance of the silicon carbide rod will also increase. The silicon dioxide film expands and contracts abnormally near the crystallization critical point (270°C). Because the temperature fluctuates at this temperature during intermittent use in batch kilns, the silica film is repeatedly broken to accelerate oxidation. Therefore, when the furnace temperature drops to room temperature, the resistance often increases sharply.
Wiring method: If the silicon carbide rods have different resistance values, the high resistance silicon carbide rods will be more concentrated when connected in series, which will easily cause the resistance of a certain silicon carbide rod to increase rapidly and shorten its life. Silicon carbide rods are generally used in combination with series and parallel connections. It is recommended to use 2 wires in series to form a group and then multiple groups in parallel. Especially when the temperature in the furnace exceeds 1350℃, it must be connected in parallel. It is recommended to use open delta wiring for three-phase wiring.