Heating tubes heated in liquids for a long time will show varying degrees of surface corrosion. The heating tube will gradually expand due to corrosion and cause leakage and eventually cause its damage to be unusable. As a user, what kind of treatment should be done to alleviate the various unfavorable results of the heating tube due to corrosion?
Causes of heating tube corrosion
Stainless steel can also rust under certain conditions. Stainless steel has the ability to resist atmospheric oxidation, that is, non-rust, and it also has the ability to resist corrosion in media containing acid, alkali and salt, that is, corrosion resistance. But the size of its corrosion resistance is changed with the chemical composition of the steel itself, the mutual state, the use conditions and the type of environmental medium. When exposed to chlorine or harsh environments, especially the passivation layer on the surface is mechanically or After chemical damage, it will rust more easily than usual. Such as 304 steel pipe, in a dry and clean atmosphere, it has absolutely excellent anti-corrosion ability, but when it is moved to the seaside area, it will quickly rust in the sea fog containing a lot of salt; while 316 steel pipe has performance good. Therefore, it is not any kind of stainless steel, which is corrosion-resistant and does not rust in any environment.
Treatment method of heating tube after being corroded
1. Chemical method:
Use spray or pickling paste to assist the re-passivation of the rusted parts to form a chromium oxide film to restore the corrosion resistance. Apply the pickling paste to the surface to be treated, the thickness of the coating film is 0.5-2mm, the general reaction time is 3-10 minutes or more, when it is used below 0℃ or where the oxide scale is thick, the time needs to be extended appropriately. It is best to use a brush to wash several times during the treatment process. After the surface oxide scale is completely removed, rinse it with clean water (lime water or alkaline water is better) to avoid returning rust. After pickling, in order to remove all contaminants and acid residues, it is very important to rinse properly with clean water. After all treatments, re-polishing with polishing equipment and sealing with polishing wax. For those with slight rust spots, you can also use a 1:1 gasoline and engine oil mixture to wipe off the rust spots with a clean cloth.
2. Mechanical method:
Sandblasting, using glass or ceramic particle shot blasting, annihilation, brushing and polishing. It is possible to use mechanical methods to wipe off the pollution caused by the previously removed materials, polishing materials or annihilation materials. All kinds of pollution, especially foreign iron particles, can become a source of corrosion, especially in humid environments. Therefore, mechanically cleaned surfaces should be properly cleaned under dry conditions. The use of mechanical methods can only clean the surface, and cannot change the corrosion resistance of the material itself. Therefore, it is recommended to re-polishing with polishing equipment after mechanical cleaning and sealing with polishing wax.
In order to let more users understand the application of heating tube materials in different corrosion-resistant liquids, we will tell you that there are mainly 304 stainless steel heating tubes, 316 stainless steel heating tubes, titanium heating tubes, Teflon heating tubes, and quartz in the market. Selection of heating tube application in corrosive environment.